What happens if a battery is inadvertently overcharged? lithium-ion is designed to operate safely within their normal operating voltage but become unstable if charged to higher voltages. When charging above 4.30V, the cell causes plating of metallic lithium on the anode; the cathode material becomes an oxidizing agent, loses stability and releases oxygen. Overcharging causes the cell to heat up. If left unattended, the cell could vent with flame.
Much attention is focused to avoid over-charging and over-discharging. Commercial lithium ion packs contain a protection circuits that limit the charge voltage to 4.30V/cell, 0.10 volts higher than the voltage threshold of the charger. Temperature sensing disconnects the charge if the cell temperature approaches 90°C (194°F), and a mechanical pressure switch on many cells permanently interrupt the current path if a safe pressure threshold is exceeded. Exceptions are made on some spinel (manganese) packs containing one or two small cells.
|