No quick answer to that.
If the part starts out in great condition, like an out of the package UE or FLM part I polish with Tripoli on a Sisal wheel then with Jewelers rouge on a soft cloth wheel. I follow that up with hand polishing using Mothers Billet polish and/or Wizzard Polish and Wizzard polished metal protector.
If the metal is anodized, has scratches or deep pits the process starts differently but ends the same way.