Originally Posted by brushlessboy16 View Post
you need carbon to harden steel...

You heat it up until it is red and non magnetic (going to have to check) then clench it in oil. then heat it back up and clench in water.

Using just water DOES case harden but not as well as added carbon.


See here
http://www.technologystudent.com/equip1/heat2.htm

where would i get this type of carbon?

i think i am just gonna leave this to a professional shop to do but just curious.

is the hardening process what gives it that black coating? cuz that i show my other mod1.5 gears are.


Jammin SCRT10 Neu 1512 1y
Losi Ten-T SCT conversion Neu 1512 1y
   
Reply With Quote
 


Currently Active Users Viewing This Thread: 2 (0 members and 2 guests)
 
Thread Tools
Display Modes Rate This Thread
Rate This Thread:

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is On

Forum Jump







Powered by vBulletin® Version 3.8.11
Copyright ©2000 - 2026, vBulletin Solutions Inc.
vBulletin Skin developed by: vBStyles.com