Guest
|
solder -
06.23.2009, 09:26 PM
so i did a search for solder and came up with 20 pages. so what solder % and type is everyone using for motor and batteries
that is all
thank you
|
|
|
|
|
|
|
|
Guest
|
06.23.2009, 11:18 PM
I use 60/40 Rosin Core from RadioShack.
|
|
|
|
|
|
|
|
RC-Monster Admin
Offline
Posts: 14,609
Join Date: Nov 2005
Location: Des Moines, IA
|
06.24.2009, 12:55 AM
Yep, that's what I use too...
|
|
|
|
|
|
|
|
RC-Monster RC8T
Offline
Posts: 2,554
Join Date: Jan 2008
Location: Syracuse, New York (Camillus)
|
06.24.2009, 01:00 AM
me 3, but not from radio shack
RC-Monster RC8T 1515 2.5D/MMM/5s RC-M 4500mah
SC10 MMPro 13.5T 2s NeuEnery 5000mah
RC18T Mamba 25/5400kv 2s lipo + 6s NiMh
|
|
|
|
|
|
|
|
Check out my huge box!
Offline
Posts: 11,935
Join Date: Aug 2007
Location: Slidell, LA
|
06.24.2009, 01:43 AM
Ditto on the 60/40. I got mine form the hardware store. Make sure you get electrical solder, not plumbing. I also picked up some silver bearing solder, but I have not tried it yet. Supposedly it melts at higher temperatures and cools of nice and shiny. Neither seem to be necessary fro what I am doing...
|
|
|
|
|
|
|
|
RC-Monster Admin
Offline
Posts: 14,609
Join Date: Nov 2005
Location: Des Moines, IA
|
06.24.2009, 01:47 AM
lol, yeah. Plumbing solder is usually acid core. Not good at all for electronics work!
|
|
|
|
|
|
|
|
Guest
|
06.24.2009, 07:00 PM
so any 60/40 is good with rosin core. what is the main difference between 60/40 and 70/30 i know its tin to lead ratio so more tin is stronger, but melts at a higher temp?.
so basically 60/40 is 60/40 no matter what brand, or are their quality differences.
|
|
|
|
|
|
|
|
Soldermaster Extraordinaire
Offline
Posts: 4,529
Join Date: Apr 2007
Location: Plymouth, MA, USA
|
06.24.2009, 07:23 PM
The 60/40 is fine for 90% of general electronics jobs (r/c included). I have some of the silver bearing solder as well. It does have a higher melting point and so you might need a higher wattage soldering iron/gun. The advantage to the SBS is that it has less resistance than the standard 60/40 and it makes a much stronger joint when it cools- both due to the silver content.
|
|
|
|
|
|
|
|
Guest
|
06.24.2009, 09:12 PM
so sbs is harder to use but better results?
|
|
|
|
|
|
|
|
Soldermaster Extraordinaire
Offline
Posts: 4,529
Join Date: Apr 2007
Location: Plymouth, MA, USA
|
06.24.2009, 09:20 PM
Yes. It's also more expensive. Again, due to the silver.
|
|
|
|
|
Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
|
|
|
Posting Rules
|
You may not post new threads
You may not post replies
You may not post attachments