Quote:
Originally Posted by What's_nitro?
I'm thinking the Rustler. I'll be making 2 6s1p packs from them. Does anyone have a link to some oxygen-free fine copper mesh? I want to use that to solder the cells. Battery bars hold too much heat so I'm afraid I wont get a good connection.
|
You're basically looking for copper braid, right?
http://www.hobby-lobby.com/copper_br..._2847_prd1.htm
I've used LOTS of this stuff, but I use it 2 rows at a time (two pieces for each end of a cell). Has worked great!
SH Z-Car, Custom Crawler, 8s Savage,
12s XTM XLB 1/7 buggy,
4wd 4-link rear/IFS Pro4 truck,
Custom Hyper 10 Short Course,
Belt-Drive Mammoth ST 1/8 truggy, 4s 17.5 MM Pro HPI Blitz